| Availability: | |
|---|---|
| Quantity: | |
| Hastelloy C-276 (UNS 10276 / W.Nr.2.4819 / NS336) | |||
| Chemical Composition % | Ni: Margin | Cr: 14.5-16.5 | Fe: 4-7 |
| W: 3-4.55 | Mo: 15-17 | Mn: ≤1 | |
| Co: ≤2.5 | C: ≤0.01 | Si: ≤0.08 | |
| P: ≤0.04 | S: ≤0.03 | V: ≤0.35 | |
| Melting Point ℃ | 1325-1370 | ||
| Density g/cm3 | 8.9 | ||
| Executive Standards | ASTM: B575 | ||
| Application Area | Bleaching containers, equipment and components operating in acidic gas environments, reactors for acetic acid and acidic products, and sulfuric acid condensers in the pulp and paper industry | ||
Designations: AWS 054
Specifications: ASTM B574 , ASTM B575 , ASTM B619
Alloy Details
| Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
| 8.89 g/cm³ | 1370 °C | 11.2 μm/m °C (20 – 100 °C) | 78.6 kN/mm² | 205.5 kN/mm² |
| 0.321 lb/in³ | 2500 °F | 6.2 x 10-6 in/in °F (70 – 212 °F) | 11400 ksi | 29806 ksi |
Heat treatment of finished parts
| Condition as supplied by AWI | Type | Temperature | Time | Cooling |
| Annealed or Spring Temper | Stress Relieve | 400 – 450 °C (750 – 840 °F) | 2 Hr | Air |
Properties
| Annealed | ||
| Approx. tensile strength | <1050 N/mm² | <152 ksi |
| Approx. operating temperature depending on loading and environment | -200 to +400 °C | -330 to +750 °F |
| Spring Temper | ||
| Approx. tensile strength | 1300 – 1700 N/mm² | 189 – 247 ksi |
| Approx. operating temperature depending on loading and environment | -200 to +400 °C | -330 to +750 °F |