| Inconel 601(UNS N06601 / W.Nr.2.4851) | |||
| Chemical composition % | Ni: 58-63 | Cr: 21-25 | Fe: Margin |
| Mn: ≤1.5 | Cu: ≤1.0 | Al: 1-1.7 | |
| C: ≤0.10 | Si: ≤0.5 | P: ≤0.03 | |
| S: ≤0.015 | |||
| Melting Point ℃ | 1320-1370 | ||
| Density g/cm3 | 8.1 | ||
| Executive Standards | ASTM: B168 | AMS: 5870 | |
| Application Area | Pallets, fixtures, high-speed gas burners, mesh belts in industrial furnaces; | ||
Designations: AWS 011
Specifications: ASTM B166
Alloy Details
| Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
| 8.11 g/cm³ | 1411 °C | 13.75 μm/m °C (20 – 100 °C) | 81.2 kN/mm² | 206.5 kN/mm² |
| 0.293 lb/in³ | 2571 °F | 7.6 x 10-6 in/in °F (70 – 212 °F) | 11777 ksi | 29951 ksi |
Heat treatment of finished parts
| Condition as supplied by AWI | Type | Temperature | Time | Cooling |
| Annealed or Spring Temper | Stress Relieve | 480 – 870 °C (900 – 1600 °F) | 1hr | Air |
Properties
| Annealed | ||
| Approx. tensile strength | < 900 N/mm² | < 131 ksi |
| Approx. operating temperature depending on loading and environment | -200 to +1000 °C | -330 to +1830 °F |
| Spring Temper | ||
| Approx. tensile strength | 1200 – 1450 N/mm² | 174 – 210 ksi |
| Approx. operating temperature depending on loading and environment | -200 to +1000 °C | -330 to +1830 °F |