| Availability: | |
|---|---|
| Quantity: | |
| Hastelloy B-3 | |||
| Chemical Composition % | Ni: ≥65 | Cr: 1.0-3.0 | Fe: 1.0-3.0 |
| W: ≤3.0 | Mo: 27-32 | Cu: ≤0.2 | |
| Mn: ≤3.0 | Co: ≤3.0 | Ti: ≤0.2 | |
| Al: ≤0.5 | C: ≤0.01 | Si: ≤0.1 | |
| P: ≤0.03 | S: ≤0.01 | V: ≤0.2 | |
| Melting Point ℃ | 1370-1418 | ||
| Density g/cm3 | 9.22 | ||
| Application Area | It has extensive applications in the fields of chemistry, petrochemicals, energy manufacturing, and pollution control. Especially in industries such as sulfuric acid, hydrochloric acid, phosphoric acid, and acetic acid | ||
Designations: AWS 051
Specifications: ASTM B335 , ASTM B619
Alloy Details
| Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
| 9.22 g/cm³ | 1418 °C | 10.6 μm/m °C (20 – 100 °C) | 83 kN/mm² | 216 kN/mm² |
| 0.333 lb/in³ | 2585 °F | 5.7 x 10-6 in/in °F (70 – 212 °F) | 12038 ksi | 31329 ksi |
Heat treatment of finished parts
| Condition as supplied by AWI | Type | Temperature | Time | Cooling |
| Annealed or Spring Temper | Stress Relieve | 400 – 450 °C (750 – 840 °F) | 2 Hr | Air |
Properties
| Annealed | ||
| Approx. tensile strength | <1200 N/mm² | <174 ksi |
| Approx. operating temperature depending on loading and environment | -200 to +400 °C | -330 to +750 °F |
| Spring Temper | ||
| Approx. tensile strength | 1600 – 2000 N/mm² | 232 – 290 ksi |
| Approx. operating temperature depending on loading and environment | -200 to +400 °C | -330 to +750 °F |