| Availability: | |
|---|---|
| Quantity: | |
| Monel K-500(UNS N05500) | |||
| Chemical Composition % | Ni: ≥63 | Fe: ≤2.0 | Cu: 27-33 |
| Mn: ≤1.5 | Ti: 0.35-0.85 | Al: 2.5-3.15 | |
| C: ≤0.25 | Si: ≤0.5 | S: ≤0.01 | |
| Melting Point ℃ | 1288-1343 | ||
| Density g/cm3 | 8.89 | ||
| ExecutiveStandards | ASTM: B127 | ASME: SB127 | AME: 4544 |
| Application Area | Turbine blades and gas turbine blades with operating temperatures below 750 ℃ on aircraft engines, fasteners, springs on ships, pumps, valves on chemical equipment, etc | ||
Designations: AWS 041
Specifications: ASTM B865
Alloy Details
| Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
| 8.44 g/cm³ | 1350 °C | Coefficient of Expansion 13.7 μm/m °C (20 – 100 °C) | 66 kN/mm² | 179 kN/mm² |
| 0.305 lb/in³ | 2460 °F | 7.6 x 10-6 in/in °F (70 – 212 °F) | 9573 ksi | 25962 ksi |
Heat treatment of finished parts
| Condition as supplied by AWI | Type | Temperature | Time | Cooling |
| Annealed | Age Harden | 580 – 590 °C (1075 – 1095 °F) | 8 – 10 Hr | Air |
| Annealed or Spring Temper | Age Harden | 530 – 540 °C (985 – 1005 °F) | 4 – 6 Hr | Air |
Properties
| Annealed | ||
| Approx. tensile strength | <850 N/mm² | <123 ksi |
| Approx. operating temperature | -100 to +260 °C | -150 to +500 °F |
| Annealed + Aged | ||
| Approx. tensile strength | >950 N/mm² | >138 ksi |
| Approx. operating temperature | -100 to +260 °C | -150 to +500 °F |
| Spring Temper | ||
| Approx. tensile strength | 1000 – 1300 N/mm² | 145 – 189 ksi |
| Approx. operating temperature | -100 to +260 °C | -150 to +500 °F |
| Spring Temper + Aged | ||
| Approx. tensile strength | 1200 – 1500 N/mm² | 174 – 218 ksi |
| Approx. operating temperature | -100 to +260 °C | -150 to +500 °F |